Note:
- Insulate with VITA Modisol again before placing on the model. This way, any material applied in the basal area will not stick to the model.
- Make corrections of the shape starting from the cervical area with OPAQUE DENTINE / DENTINE and ENAMEL.
It appears that you are currently in United States.
United States
Please select treatment/processing step and get the corresponding product overview.
Please select treatment/processing step and get the corresponding product overview.
Based on the poor thermal conductivity of both materials (Y-TZP and veneering ceramic), higher residual stress can occur in this compound system than is known to typically occur in metal ceramics. This residual thermal stress in the veneering ceramic can be counteracted by means of slow cooling during the last firing cycle to below the transformation temperature of the veneering ceramic (for VITA LUMEX AC, approx. 550 °C).
VITA Zahnfabrik
H. Rauter GmbH & Co. KG
Postfach 1338
D-79704 Bad Säckingen
Phone+49 7761 562 0
Fax+49 7761 562 299
info@vita-zahnfabrik.com